![]() The crystallographic texture intensity and surface roughness increased as the part thickness decreased for 90 deg and increased for 45 deg build angle. ![]() A preferred 〈100〉 crystallographic orientation was found along the build direction in all cases. Hence, thin-walled IN-939 structures of different thicknesses (0.5, 1 and 2 mm) were manufactured at two build angles (90 and 45 deg) by PBF-LB/M. Powder bed fusion-laser beam of metals (PBF-LB/M) has attracted significant interest due to the possibility of producing dedicated design features like thin-walled structures, even though their mechanical response and microstructure are not well understood.